ASTM D6186 - Oxidation Induction Time of Lubricating Oils by Pressure Differential Scanning Calorimetry (PDSC)
Significance and Use
1.1 This test method covers the determination of oxidation induction time of lubricating oils subjected to oxygen at 3.5 MPa (500 psig) and temperatures between 130 and 210°C.
Scope
1.1 This test method covers the determination of oxidation induction time of lubricating oils subjected to oxygen at 3.5 MPa (500 psig) and temperatures between 130 and 210°C.
Extracted, with permission, from ASTM D6186-19 - Oxidation Induction Time of Lubricating Oils by Pressure Differential Scanning Calorimetry (PDSC), copyright ASTM International, 100 Barr Harbor Drive, West Conshohocken, PA 19428. A copy of the complete standard may be purchased from ASTM International, astm.org